Skip to content
PlanarManufacturing Wiki

Splines

Shaft/hub spline geometry, fit, engagement and inspection, with bounded standard and catalogue references.

Tags: parts-and-design, splines, shafts, power-transmission

Research draft — not customer-confirmed

On this page

Define the connection

A mechanical spline uses repeated mating teeth and spaces to connect a shaft and hub rotationally. The connection may permit axial sliding or hold a fixed axial position depending on its design. This reference concerns shaft/hub connections, not mathematical spline curves or meshing gear pairs.

Parallel straight-sided and involute splines are different geometry families. AGMA's publications catalogue lists AGMA 945-1-B20 and 945-2-B20 as design/application information sheets covering both families, with the second addressing inch-based splines. Their scope includes geometry, fits, materials, manufacture, rating, inspection, lubrication and failure. A tooth count and outside diameter are therefore only part of specifying a connection. AGMA publications catalogue, spline information sheets

Standard family and fit come first

DIN 5480 concerns involute splines based on reference diameters. Its public Part 2 scope describes detachable, sliding or fixed shaft/hub connections, a 30° pressure angle, normally flank centering, exceptional diameter centering, and a fit system that accounts for effective form deviations. Do not assume every involute spline uses that pressure angle or those fits. DIN 5480-2:2025-10 scope

The public DIN record identifies DIN 5480-1:2026-05 as a corrected edition following the October 2025 document. Preserve the actual required part and edition on the drawing; a catalogue based on an earlier standard is not evidence of conformance to every subsequent correction. Public metadata does not replace the full standard's dimension and inspection rules. DIN 5480-1:2026-05

Requirement Information to keep explicit
Geometry family Governing standard/edition, internal versus external member, tooth count and profile
Size Module or pitch system, pressure angle, reference and limiting diameters
Fit Tooth/space tolerance classes, centering basis and required axial motion
Engagement Useful contact length, entry chamfers, runouts and axial retention
Acceptance Datums, inspection method, processing/finishing state and functional requirements

Separate axial retention from torque transmission. A connection that slides together successfully has not thereby demonstrated the required load capacity or retention. Establish fit from the complete paired definitions rather than matching a nominal diameter alone.

Read a catalogue designation carefully

Ondrives' splined-shaft/bushing catalogue, printed Updated May 2022, shows an external shaft designation 48x2.00x30x22x8f. Its diagram identifies reference diameter, module, pressure angle, tooth count and tooth-thickness/tolerance information; the table lists this as a 48 mm reference-diameter, module 2, 22-tooth shaft. The shaft heading specifies DIN 5480 W 8f slide fit. These are that product family's definitions, not a complete generic substitution rule. Ondrives precision splined shafts and bushings, shaft page

Original geometry check: for an assumed straight involute spline with module m = 2 mm and z = 22, the pitch diameter is d = mz = 44 mm, angular tooth spacing is 360/22 ≈ 16.364°, and circular pitch is πm ≈ 6.283 mm. The catalogue's 48 mm reference diameter is consequently not interchangeable with this calculated pitch diameter. Neither number should be substituted for a major/minor limit diameter or an inspection dimension without its governing definition.

These calculations describe ideal spacing only. They do not generate a complete DIN profile, tooth-thickness limits, measuring-pin size or a mating part. Use the applicable standard and controlled drawings for those values.

Manufacture and load review

Specify the material, condition, heat treatment and final contact surfaces. Agree how the manufacturing process will reach an internal or external profile, particularly near a shoulder or blind end. Show any required runout or relief as actual geometry, and distinguish overall tooth length from useful engagement after chamfers and incomplete end profiles.

For a proposed connection, review torque and its reversals, contact distribution, engagement, alignment, surrounding shaft/hub section, lubrication and wear conditions. Do not divide total load equally among all teeth and treat that assumption as an established rating. AGMA's scope explicitly treats rating, lubrication and failure alongside geometry; a supplier's dimension table is insufficient for those separate decisions. AGMA spline design/application scope

Any change to tooth form, runout, hardening or surface finish needs review against both assembly and operating requirements. A relief that solves tool access can reduce the remaining section; a tighter fit can change assembly and sliding behavior.

Inspection is more than outside diameter

Gleason offers go/no-go rings and plugs, variable spline gauges and setting masters. Its variable indicator gauges can report effective and actual tooth thickness or space width. Those are distinct measurement quantities; specify the intended method and limits instead of asking only for a caliper reading across the outside. Gleason functional and electronic gauges

As a proposed receiving sequence, confirm identification and standard, check required dimensions/profile and datums, apply the agreed functional/variable inspection, inspect usable engagement and edge condition, and verify assembly requirements. Keep gauge calibration and the inspected processing stage with the record. A successful trial fit of one pair does not establish interchangeability across all permitted production limits.

Source scope

Reviewed on the date above. DIN edition dates are taken from the publisher's records; Ondrives prints May 2022. The live Gleason page has no verified technical revision date. AGMA catalogue descriptions are used for scope, not as a replacement for the design methods themselves. Calculations and proposed review/receiving checks are editorial guidance under stated assumptions.

Part features