  • UNS C10100 copper

    Specify oxygen-free electronic copper by product standard, form and temper; interpret purity, conductivity and processing data without transferring supplier values across conditions.

  • UNS C11000 copper

    Specify electrolytic tough-pitch copper by product form, temper, conductivity and oxygen-sensitive processing requirements.

  • UNS C12200 copper

    Specifying phosphorus-deoxidized C12200 by product form, temper, conductivity basis, joining route and service requirements.

  • UNS C14500 copper

    Specify tellurium copper by product standard, form and temper; interpret machining ratings, conductivity and joining guidance without transferring them to finished-part guarantees.

  • UNS C17200 copper alloy

    Select copper-beryllium by product form, temper, aging route and conductivity, with process-specific beryllium exposure controls.

  • UNS C26000 brass

    Selecting cartridge brass by supplier chemistry, product form, temper, forming direction and corrosion exposure.

  • UNS C28000 brass

    Specify Muntz metal by chemistry, product standard and condition; distinguish CuZn40 supplier examples from UNS compliance and qualify forming, joining and corrosion service.

  • UNS C36000 brass

    Specify free-cutting leaded brass by product form, temper and acceptance limits; distinguish machining performance from corrosion and compliance suitability.

  • UNS C46400 brass

    Specifying uninhibited naval brass by chemistry, product form, temper, test basis and marine exposure requirements.

  • UNS C51000 bronze

    Specify 5% tin phosphor bronze by form and temper; interpret spring, fatigue, conductivity and fabrication data with their stated conditions.

  • UNS C63000 bronze

    Specify wrought nickel-aluminum bronze by product standard, size and temper; qualify heat treatment, bearing duty and corrosion exposure separately.

  • UNS C93200 bronze

    Selecting leaded tin bearing bronze by casting route, property basis, lubrication system and finished-component requirements.

  • UNS C95400 bronze

    Specify cast aluminum bronze by casting standard, delivered condition and acceptance tests; distinguish C95400 and heat-treated product data from finished bearing or structural capability.

Read Markdown