# Strip stock

Strip material identity, temper, edge and shape requirements, coil formats and usable-length accounting.

Reviewed: 2026-11-01

Tags: materials, stock-forms, strip, coil

## Strip is a product description, not a grade

A **100.0 m strip coil** with assumed exclusions of **1.0 m at the ends** and **0.2 m at a joint** leaves **98.8 m**. At **40.0 mm pitch**, that is **2,470 pitches** before setup scrap, rejects and trim. Apply the exclusions only if they are outside the supplier's certified usable length.

Strip stock is flat material supplied in a specified width and thickness, commonly as coils or cut lengths for further processing. Its exact distinction from sheet depends on the product specification and material family. Do not apply one universal width boundary to carbon steel, stainless steel, copper alloys and aluminum.

For a bounded steel example, **ASTM A109/A109M-25** covers cold-rolled carbon steel strip with specified temper, edge or finish, in coils or cut lengths. Its public scope limits specified carbon to 0.25% maximum and distinguishes strip from sheet and high-carbon strip. Products with strip tolerances wider than its normal range may be agreed, while technically classified as sheet. This is a standard-specific distinction, not a universal definition of strip. [ASTM A109/A109M-25, public scope](https://store.astm.org/a0109_a0109m-25.html)

Keep material specification/edition, grade, temper or delivery condition, dimensions, edge, surface and packaging as separate records. A description such as “spring strip, 0.5 mm” leaves both material and acceptance requirements unresolved.

## Rolling, slitting and supplied condition

A strip's width may result from longitudinal slitting; its final thickness and mechanical state may involve rolling and heat treatment. These operations answer different questions. Precision slitting does not itself certify the material's strength or temper, and bright appearance does not establish an annealed state.

Elgiloy Specialty Metals separately lists precision rolling, precision slitting, edge finishing and coil tempers. Its stated delivery forms include pancake coils, block coils, spools and reels. Its capability chart explicitly warns that not all thicknesses are available at maximum width. Use it as a named producer example rather than assuming every alloy/size/temper combination is available. The webpage has no verified technical revision date. [Elgiloy strip and foil capabilities](https://www.elgiloy.com/strip-division/capabilities)

Outokumpu's precision-strip offering likewise distinguishes targeted strength, grain size, surfaces and edge options. Its listed dimensional envelope is not a guarantee that all combinations are produced in every grade. The undated live page lists austenitic and ferritic grades commonly, with other families available on request. [Outokumpu precision strip](https://www.outokumpu.com/en/products/flat-products/precision-strip)

## Dimensions, tolerances and shape

| Requirement | Question to resolve |
|---|---|
| Thickness | Nominal or minimum basis; tolerance class and measurement location? |
| Width | Slit or other edge; dimensional tolerance and treatment allowance? |
| Straightness/camber | Deviation over what reference length and under what conditions? |
| Flatness | Permitted edge wave, internal buckle, coil set and cross bow? |
| Length and format | Coil mass, dimensions, usable length, joints and end condition? |

Alleima's *Precision Strip Steel* brochure treats waviness, coil set and cross bow as different shape deviations. Its straightness tables also distinguish hardened-and-tempered from cold-rolled conditions. No independently verified printed edition date was found, so the brochure's numerical limits are not adopted here as generic tolerances. [Alleima precision-strip brochure, shape section](https://www.alleima.com/siteassets/documents/strip/precision_strip_steel_brochure_fin.pdf)

Specify the reference length and support arrangement for shape measurement. Keep the width/thickness class and original units with each tolerance.

ASTM A109/A109M-25 specifies that its inch-pound and SI systems are separately standard; its metric tolerance values are not necessarily exact conversions of customary values. Retain the ordered system rather than mixing limits from the two sets of tables. [ASTM A109/A109M-25, unit-system provisions](https://store.astm.org/a0109_a0109m-25.html)

## Edges are an explicit selection

Alleima defines a **slit edge** as one made by circular shearing with the shearing burr not removed. A **deburred edge** removes that burr; a **round edge** is a separate profile. These terms should not be merged into a single “finished edge” field. Availability depends on grade, size and tolerance, rather than merely the requested profile name. No technical issue date was verified on the cited page. [Alleima strip edges](https://www.alleima.com/en/products/strip-steel/edges/)

Specify burr direction/limit, required edge profile and inspection when they affect feeding, contact, bending or the finished component. An edge treatment can alter the usable width, so coordinate it with dimensional acceptance. Obtain the supplier's drawing or agreed profile for a critical edge rather than inferring it from a photograph.

## Surface, coil format and continuous feed

Outokumpu's buying guide discusses glossy/matt surfaces, deburred or rounded edges, customized packaging and spools/coils. It explains that its “endless” strip may join individual coils by welding after rolling to support continuous feeding. Therefore “endless” does not mean joint-free material. The article is hosted in its 2023 expertise collection; no separate revision date was verified. [Outokumpu precision-strip buying guide](https://www.outokumpu.com/en/expertise/2023/buying-precision-strip-here-are-the-most-important-points-to-think-about)

An order for an automatic line should define acceptable coil inside/outside diameter, mass, winding arrangement, orientation, joints and joint marking. Agree how ends and joins are handled by the process. Packaging also needs to suit unloading, storage and the intended cleanliness; nominal coil length alone does not establish continuous usable production length.

Surface acceptance should describe the actual requirement: finish, roughness if needed, permitted defects, lubrication, coating and cleanliness. Preserve which side faces the tooling or becomes visible. A surface suitable for one stamping operation may require additional preparation for bonding, welding or coating.

## Original usable-length estimate

**Illustrative assumptions:** a 100.0 m strip coil feeds single-lane blanks at a constant 40.0 mm pitch. Assume 1.0 m total is excluded for leading/trailing ends and a further 0.2 m is excluded around a marked joint. These are planning assumptions, not supplier allowances.

Usable length = 100.0 − 1.0 − 0.2 = **98.8 m**. At 0.040 m per pitch, the geometric maximum is **2470 pitches**, compared with 2500 from the gross length. The exclusions account for 30 pitches, or **1.2%** of gross pitch count. This excludes setup scrap, rejected parts and any additional trim or interruptions. Actual accepted output requires the real process yield and joint policy.

## Ordering and acceptance

1. Define material standard/edition, grade, condition and required mechanical properties.
2. Agree dimensions, tolerance classes, shape, surface and edge requirements.
3. Match coil format, winding, joint policy and packaging to the production line.
4. Inspect agreed characteristics and retain heat/lot identity through slitting and cutting.
5. Qualify the actual forming/joining route and accept finished components separately.

Source-specific envelopes and marketing application lists are discovery aids. A usable purchase record identifies what is contractually required, what was supplied and what downstream processing changed.