# VCI packaging

Vapor corrosion inhibitor packaging: metal compatibility, enclosure design, preparation and bounded protection claims.

Reviewed: 2026-11-01

Tags: delivery, packaging, corrosion

## What VCI contributes

Vapor corrosion inhibitor (VCI) from treated paper, film or an emitter must reach exposed metal. A breach or sustained airflow can defeat the enclosure, and existing corrosion remains. [ZERUST, VCI FAQ: mechanism, moisture and already-corroded parts](https://www.zerust.com/faq/)

These functions may be combined in one construction, but they are not interchangeable. Daubert's packaging-design examples use separate VCI sources, plain-poly enclosures and, for one overseas machinery arrangement, an additional heat-sealed barrier. The same presentation shows how corrugated separators can obstruct inhibitor access to bare metal. Treat the complete arrangement as the preservation system. [Daubert Cromwell, Packaging Design Considerations, slides 7–8, 12 and 17–18; undated](https://daubertcromwell.com/wp-content/uploads/PackagingDesignConsiderations.pdf)

The packaging has several distinct jobs:

| Element | Intended function | What needs specifying |
| --- | --- | --- |
| VCI source | Deliver chemistry appropriate to the metal | Product/formulation, quantity, placement and enclosure |
| Barrier | Limit ingress or loss through the package | Material, seams, closures and damage resistance |
| Desiccant, if used | Adsorb water vapor | Moisture load, capacity and placement |
| Cushioning and supports | Prevent handling damage and movement | Contact materials, restraints and load path |

## Match the chemistry to the actual surfaces

“VCI” describes a class of technology, not one interchangeable chemical. Daubert identifies metal type, inhibitor formulation and loading, carrier, moisture behavior and shipping/storage conditions as selection variables. A formulation successful in one application may fail in another. Ask for compatibility with the actual alloys, plated surfaces and process residues rather than accepting a generic “metal protection” description. [Daubert Cromwell, Selecting the Right VCI](https://daubertcromwell.com/vci-education/selecting-the-right-vci/)

A useful application description includes each exposed metal, mixed-metal contacts, surface treatment, protective oil or coolant residue, cleaning process and intended next operation. Include seals, plastics, labels, adhesives and electronics present in an assembly when requesting compatibility review. Verify that the selected treatment is acceptable before painting, bonding, welding or precision cleaning; a favorable claim for one VCI formulation does not qualify all downstream processes.

Do not identify the chemistry by bag color. For example, ZERUST's **ICT510-C VCI Bags** sheet lists ferrous, multimetal, non-ferrous and anti-tarnish formulations, with several typical colors and optional additives. Specify the ordered formulation and construction in the packaging instruction. [ZERUST ICT510-C technical data sheet, revision A4, page 1](https://www.zerust.com/resourcefiles/infosheets/zerust-ict-vci-bags-technical-data-sheet/)

## Prepare the parts and control handling

VCI does not remove standing water. Wet parts can corrode before protection develops; protection depends on inhibitor reaching the surface and on conditions inside the package. Existing corrosion also remains present. Preparation therefore needs its own acceptance criterion rather than relying on the bag to correct an upstream problem. [ZERUST, VCI FAQ: wet parts and protection establishment](https://www.zerust.com/faq/)

Daubert's illustrated operating guidance calls for gloves when handling bare metal, complete coverage, closure of the VCI bag, and separation from cardboard, corrugated boxes and wooden pallets. It also directs operators to return unused sheets to their box rather than leaving stock exposed. These are practical controls against contamination and loss of packaging effectiveness. [Daubert Cromwell, VCI Packaging Guidelines; undated](https://daubertcromwell.com/wp-content/uploads/VCI-Packaging-Guidelines-English_v4.pdf)

Define what “clean and dry” means for the part and process: residual wash liquid in holes, fingerprints, chips and an incompatible residue are different conditions. The packing record should identify the part condition and any approved supplementary preservative. Avoid transferring a damp part directly into a closed pack simply because its exposed face looks dry.

## Enclosure, placement and access

Inhibitor must reach the surfaces requiring protection. A large outer bag does not demonstrate that a tightly packed stack, isolated cavity or wrapped subassembly has adequate access. Draw the enclosure boundary and identify every internal barrier and layer.

For **Daubert Cromwell materials specifically**, its European guidance says the unprinted paper face should face the metal and gives a maximum 12-inch source-to-metal distance. It also provides coverage rules based on both metal surface area and void volume and recommends compatibility testing. These are supplier guidelines to confirm for the chosen product, not universal VCI dimensions or a substitute for evaluating a complex pack. [Daubert Europe, Guidelines for Use](https://dauberteurope.eu/vci-education/guidelines-for-use/)

As an **original design-review example**, consider steel discs stacked inside a lined crate with corrugated separators. Review both faces of the inner discs, not just the distance from the outer liner to the stack. Identify whether separators obstruct the vapor path or introduce a problematic contact material, then obtain an approved interleaving and closure arrangement. Changing the number of layers changes the arrangement being qualified even when the crate dimensions stay the same.

The bag instruction should state closure method, puncture prevention, inspection access and resealing procedure. Daubert's guidance permits opening and resealing its packages while avoiding contact with the metal, but this should not be interpreted as permission for indefinitely open storage. [Daubert Europe, Guidelines for Use](https://dauberteurope.eu/vci-education/guidelines-for-use/)

## Combining VCI and desiccant

A manufacturer can specify a combined system. ZERUST's **ZDC Desiccants**, revision A1, describes clay desiccant for reducing humidity inside an enclosure and use with ZERUST VCI products. It requires keeping a ZDC pouch away from direct metal contact and securing it against movement; when used with named VCI diffusers, the desiccant and diffuser are kept apart. Its layered-package guidance also addresses desiccant placement within layers. This supports a designed combination, not arbitrary mixing of inhibitors and drying agents. [ZERUST ZDC technical data sheet, pages 1–2](https://www.zerust.com/resourcefiles/infosheets/zerust-zdc-desiccants-technical-data-sheet/)

Specify each component separately. The bag's inhibitor loading is not a desiccant capacity, and adding a drying pouch does not establish a known moisture budget. Barrier permeation, enclosed moisture and package opening still matter. Keep unused desiccant sealed until needed and follow its own storage and handling instructions. [ZERUST ZDC technical data sheet, operating summary](https://www.zerust.com/resourcefiles/infosheets/zerust-zdc-desiccants-technical-data-sheet/)

## Read protection and storage claims carefully

The ICT510-C revision A4 sheet calls for clean, dry parts near room temperature, tightly closed packages and additional interleaving for larger or layered packs. It describes correct indoor use but explicitly does **not recommend outdoor protection**. Its unused-product storage instruction is up to three years from shipment in original packaging, cool, dry and away from sunlight. That inventory period is not a three-year guarantee for packaged parts. The PDF identifies its revision but prints no calendar revision date. [ZERUST ICT510-C technical data sheet, pages 1–2](https://www.zerust.com/resourcefiles/infosheets/zerust-ict-vci-bags-technical-data-sheet/)

Qualify a proposed protection period against a defined route and storage environment. Record metal and finish, preparation, product revision, enclosure and interleaving, anticipated openings, temperature/humidity exposure and corrosion acceptance criteria. Inspect representative packed parts after relevant exposure and agree how damage or delayed storage changes disposition. Avoid translating a laboratory result or a conditional “years” claim into a universal shelf life.

Unpacking ends the controlled enclosure. Plan subsequent handling and storage as a separate preservation stage; do not assume the temporary inhibitor atmosphere continues protecting a part indefinitely after removal. [ZERUST, VCI FAQ: protection after removal](https://www.zerust.com/faq/)

## Related references

[Desiccant packaging](./desiccant-packaging.md) · [Interleaving sheets](interleaving-sheets.md) · [Delivery guides](../index.md)