# Self-clinching nuts

How sheet-metal clinching retains a threaded nut, with bounded PEM examples for holes, sheet thickness, hardness, material and finish.

Reviewed: 2026-10-30

Tags: components, fasteners, sheet-metal

PEM's **SP-M3-1**, intended for stainless receiving sheet, lists **M3 × 0.5**, **1.00 mm** minimum sheet, a **4.22 +0.08 mm** mounting hole and sheet hardness up to **HRB 90 / HB 185**. The stainless **CLS-M3-1** instead lists **HRB 70 / HB 125** and belongs to the steel-or-aluminum-sheet family. Select by host material, hardness and shank code as well as thread. [SP-M3-1](https://catalog.pemnet.com/item/nuts-types-s-ss-cls-clss-cla-sp/self-clinching-nuts-types-s-ss-cls-clss-sp-metric/sp-m3-1), [CLS-M3-1](https://catalog.pemnet.com/item/nuts-types-s-ss-cls-clss-cla-sp/self-clinching-nuts-types-s-ss-cls-clss-sp-metric/cls-m3-1).

## What self-clinching means

A clinch nut is squeezed into a prepared sheet hole. Displaced host metal captures its retaining feature. [PennEngineering, self-clinching mechanism](https://www.pemnet.com/eu/engineering-services/what-is-self-clinching-technology/).

PEM identifies the knurls as displacers and the ramped shank as a retention feature. [PEM, Self-Clinching Technology](https://www.pemnet.com/eu/products-overview/self-clinching-technology/).

## Distinguish the attachment mechanisms

| Family | What forms the attachment | Why the distinction matters |
| --- | --- | --- |
| Self-clinching sheet-metal nut | Ductile sheet material moves into the nut's retaining recess. | Hole, sheet properties and clinching geometry belong to one specified fastener system. [PEM mechanism](https://www.pemnet.com/eu/products-overview/self-clinching-technology/) |
| Blind rivet nut | A setting-tool stroke forms a closing bead in the rivet-nut body. | Its deforming body and grip geometry describe a different attachment. [HONSEL, setting process](https://www.honsel.de/en/products/fasteners/blind-rivet-nuts/technical-explanations/) |
| Projection weld nut | Welding equipment joins the nut to the sheet. | PEM's WN/WNS family specifies a welding process, rather than a clinching interlock. [PEM, WN/WNS](https://catalog.pemnet.com/viewitems/weld-nuts-types-wn-wns/self-locating-projection-weld-nuts-unified) |
| Broaching fastener | Knurls cut into a brittle substrate such as a PCB and create an interference fit. | Being pressed into a hole does not make a broaching insert a ductile-sheet clinch nut. [PEM, Broaching Technology](https://www.pemnet.com/eu/products-overview/broaching-technology/) |

PEM's FAQ says ordinary self-clinching installation generally needs access to both sheet faces and a squeezing action; impact alone does not allow the required cold flow. It also identifies exceptions for some larger nuts. Those exceptions are not evidence that the M3 examples below support blind installation. [PEM FAQ, installation access and squeezing](https://www.pemnet.com/resources/faq/)

## Read the complete part designation

The following are **supplier catalog examples**, not a generic design table. All dimensions are millimeters. Each column cites the exact PEM item whose HTML specification was read; no controlled CAD drawing revision was inspected.

| Catalog field | [S-M3-1ZI](https://catalog.pemnet.com/item/nuts-types-s-ss-cls-clss-cla-sp/self-clinching-nuts-types-s-ss-cls-clss-sp-metric/s-m3-1zi) | [CLS-M3-1](https://catalog.pemnet.com/item/nuts-types-s-ss-cls-clss-cla-sp/self-clinching-nuts-types-s-ss-cls-clss-sp-metric/cls-m3-1) | [SP-M3-1](https://catalog.pemnet.com/item/nuts-types-s-ss-cls-clss-cla-sp/self-clinching-nuts-types-s-ss-cls-clss-sp-metric/sp-m3-1) |
| --- | --- | --- | --- |
| Internal thread | M3 × 0.5; ASME B1.13M, 6H | M3 × 0.5; ASME B1.13M, 6H | M3 × 0.5; ASME B1.13M, 6H |
| Shank code | 1 | 1 | 1 |
| A, maximum shank | 0.97 | 0.97 | 0.97 |
| Recommended minimum sheet thickness | 1.00 | 1.00 | 1.00 |
| Hole size, under catalog heading “+ 0.08” | 4.22 | 4.22 | 4.22 |
| Minimum hole centerline to sheet edge | 4.8 | 4.8 | 4.8 |
| Sheet hardness limit as cataloged | HRB 80 / HB 150 or less | HRB 70 / HB 125 or less | HRB 90 / HB 185 or less |
| Nut material | Heat-treated carbon steel | 300 series stainless steel | Age-hardened A286 stainless steel |
| Standard finish as cataloged | Zinc plate per ASTM B633, SC1 (5 µm), Type III, colorless | Passivated and/or tested per ASTM A380 | Passivated and/or tested per ASTM A380 |

The shank code is consequential even with the same thread: **S-M3-2ZI** lists A maximum 1.38 mm and recommended minimum sheet thickness 1.4 mm, while retaining the 4.22 mm hole listing and 4.8 mm centerline-to-edge minimum. “M3” alone therefore cannot select the shank. [PEM, S-M3-2ZI](https://catalog.pemnet.com/item/nuts-types-s-ss-cls-clss-cla-sp/self-clinching-nuts-types-s-ss-cls-clss-sp-metric/s-m3-2zi)

These fields describe separate boundaries: A is a fastener dimension; minimum sheet thickness is a host requirement; hole size is not thread diameter; centerline-to-edge distance is measured from the hole center, not its wall. The item-page footnote directs use of at least the specified centerline-to-edge value to limit sheet distortion. The HTML hole heading is reproduced above without inventing a missing lower-tolerance notation or hole-production specification. [PEM, S-M3-1ZI specifications and footnotes](https://catalog.pemnet.com/item/nuts-types-s-ss-cls-clss-cla-sp/self-clinching-nuts-types-s-ss-cls-clss-sp-metric/s-m3-1zi)

## Material and process boundaries

PEM recommends its S/SS family for steel or aluminum sheets within the stated hardness limit. Its SP item explicitly targets stainless steel sheet. A stainless **nut** designation therefore does not, by itself, identify a nut for stainless **sheet**: CLS-M3-1 and SP-M3-1 have different materials and allowable sheet-hardness listings despite matching nominal geometry. HRB and HB are the supplier's listed hardness scales, not conversion rules established here. [PEM, S family context](https://catalog.pemnet.com/item/nuts-types-s-ss-cls-clss-cla-sp/self-clinching-nuts-types-s-ss-cls-clss-sp-metric/s-m3-2zi), [PEM, SP-M3-1 application](https://catalog.pemnet.com/item/nuts-types-s-ss-cls-clss-cla-sp/self-clinching-nuts-types-s-ss-cls-clss-sp-metric/sp-m3-1)

Ductility, hardness, thickness and corrosive environment all affect the design of the clinching features. Passing one hardness limit does not establish the other conditions. [PEM, technology limitations](https://www.pemnet.com/eu/products-overview/self-clinching-technology/)

Material and finish also remain separate selections. PEM's FAQ identifies galvanic-corrosion potential for passive 300 series stainless fasteners in aluminum when electrolyte is present; acceptability depends on the application and the function of the interface. A passivation designation alone is not a corrosion-compatibility approval. [PEM FAQ, stainless fasteners in aluminum](https://www.pemnet.com/resources/faq/)

The manufacturer's mechanism illustration uses parallel punch and anvil faces. Tool access and support are therefore design inputs, but this page supplies no tooling geometry, force setting or installation sequence. [PEM, mechanism and equipment illustration](https://www.pemnet.com/eu/engineering-services/what-is-self-clinching-technology/)

## Standards and evidence boundary

AIA's **NAS/NASM Mailing 22-11**, dated November 30, 2022, lists **NASM45938/1, revision 3**, titled “Nut, Plain, Clinch (Self-Clinching, Round),” with the memo's new-revision marker. The two-page public memo was read, including its page images. It is a publication notice, not the full standard; this research does not establish its detailed requirements, current amendment state or conformity of the commercial examples. [AIA memo, pages 1–2](https://www.aia-aerospace.org/wp-content/uploads/22-11-NASC-Mailing-30-November-2022.pdf)

The supplier's ASTM and ASME references above are transcribed item attributes. Their editions are not identified by those item pages, and the full standards were not reviewed. The manufacturer HTML pages likewise expose no technical drawing revision or reliable technical publication date; their copyright footer is not treated as one.

Sources were retrieved on October 31, 2026 UTC, which was **October 30, 2026 PDT** in America/Los_Angeles; the reviewed date uses that local business date. Direct access to PEM's CL bulletin and handbook PDFs failed, and web screenshot calls did not expose usable page pixels. Their extracted text is excluded from the technical evidence used here. In particular, older PDF search results and live HTML show differing SP Brinell figures; the table preserves the exact SP-M3-1 HTML value rather than reconciling editions that were not visually inspected.

This draft establishes no universal press force, screw tightening torque, torque-out, pushout, capacity, service life, removal/reinstallation allowance or customer qualification. Hole preparation, coating sequence and production tooling remain outside its verified coverage. Those require the applicable supplier documents and evidence for the actual assembly.

## Related reference