# Choosing MicroPolish polishing media

Compare MicroPolish and MicroPolish II, powder and suspension, without confusing abrasive size with finished roughness.

Reviewed: 2026-11-02

## Choose for the specimen and the defect you need to remove

MicroPolish products are used for final metallographic specimen preparation. Begin with the specimen material, its previous preparation step and the surface needed for analysis. **Matching an abrasive-size label alone is not enough to substitute one polishing product for another.**

Buehler distinguishes agglomerated MicroPolish alumina from deagglomerated MicroPolish II. Its [final-polishing product guide](https://www.buehler.com/products/grinding-and-polishing/grinding-and-polishing-consumables/final-polishing-suspensions/) describes product families and applications. These are specimen-preparation products, distinct from a qualified production-finishing route.

## Compare the choices

| Choice | Practical distinction | Where to look next |
| --- | --- | --- |
| MicroPolish | Agglomerated alumina; powder and suspension offerings | [MicroPolish sizes and product codes](micropolish-alumina-powder.md#nominal-sizes-and-powder-codes) |
| MicroPolish II | Additional processing breaks up particle clusters; matching nominal size does not make it identical to MicroPolish | [MicroPolish II particle behavior](micropolish-ii-alumina-powder.md#deagglomeration-and-particle-size-language) |
| Dry powder | Carrier and concentration need to be specified separately | [Carrier choice](micropolish-ii-alumina-powder.md#carrier-choice-and-applicability) |
| Prepared suspension | Liquid formulation has its own identity and safety information | [Powder versus suspension](micropolish-alumina-powder.md#powder-suspension-and-micropolish-ii) |

Buehler's [technical note on oxide polishing media](https://www.buehler.com/assets/solutions/technotes/How_to_Select_and_Use_Final_Polishing_Oxide_Media.pdf) explains deagglomeration and carrier considerations. Reduced clustering is not a guarantee that all particles are below the nominal size. The detailed pages preserve product-specific and historical evidence.

## Example: scratches remain after final polishing

In an illustrative investigation, a specimen still shows scratches after a nominal 1 µm polishing step. The size label does not establish whether those scratches came from residual damage, contamination, particle clusters or the preparation sequence. Changing to another 1 µm product without checking those factors does not isolate the cause.

Compare the previous abrasive step, specimen response, cloth condition, cleaning and actual medium. A controlled comparison should keep the other preparation conditions consistent and assess the surface required by the analysis. This is an investigation structure, not a manufacturer recipe or a claim that one product will always remove the scratches.

## Three common purchasing mistakes

- **Abrasive size versus surface roughness:** a 1 µm abrasive designation is not a promise of 1 µm Ra. [Surface profilometry](../../inspection/methods/surface-profilometry.md) explains a separate measurement problem.
- **Powder versus liquid package:** a mass of powder and a volume of suspension are not equivalent purchases without formulation and concentration information.
- **Historical versus current code:** older MicroPolish II catalogs list variants whose availability and replacement history are not established by the current product page. Use the [historical-code comparison](micropolish-ii-alumina-powder.md#historical-grades-and-package-codes) when matching an older record.

## Follow the preparation into inspection

Choose the medium to support the intended examination, then assess whether preparation artifacts could affect the result. For production surface treatment, use the separate [finishing-process collection](../../processes/finishing/index.md). For product identification and handling, distinguish [technical data sheets](../../sourcing/documents/technical-data-sheets.md) from [safety data sheets](../../sourcing/documents/safety-data-sheets.md).

Reviewed November 2, 2026 PST. Manufacturer guidance supports the product distinctions. The troubleshooting example is original explanatory synthesis. No universal speed, pressure, duration, mixing concentration or guaranteed surface finish is supplied.